MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
422 Stainless Steel 540°C (1000°F) temper
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: austenitized at 1040°C for 1 hour, oil quench, temper for 2 hours

Key Words: UNS S42200, AMS 5655, ASTM A565, SAE J467, DIN 1.4935, JIS SUH 616
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1610 MPa
 1165 MPa
@Temperature 540 °C
Tensile Strength, Yield 1005 MPa
@Strain 0.2 %
 869 MPa
@Strain 0.2 %,
Temperature 540 °C
Elongation at Break 16 %in 36 mm
 16 %
@Temperature 540 °C
in 36 mm
Tensile Modulus 199.2 GPa
 141.4 GPa
@Temperature 595 °C
 166.6 GPa
@Temperature 425 °C
 189.6 GPa
@Temperature 260 °C
Poissons Ratio 0.20Calculated
Shear Modulus 62.0 GPa
@Temperature 593 °C
 72.4 GPa
@Temperature 427 °C
 79.3 GPa
@Temperature 260 °C
 82.7 GPa
@Temperature 23.9 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.2 µm/m-°C
@Temperature 0.000 - 100 °C
 11.3 µm/m-°C
@Temperature 0.000 - 315 °C
 11.9 µm/m-°C
@Temperature 0.000 - 540 °C
 12.1 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 23.9 W/m-K
@Temperature 100 °C
 27.3 W/m-K
@Temperature 500 °C
Melting Point 1470 - 1480 °C
Solidus 1470 °C
Liquidus 1480 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 - 0.25 %
Chromium, Cr 12 %
Iron, Fe 84 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 1.0 %
Nickel, Ni 0.75 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.025 %
Tungsten, W 1.0 %
Vanadium, V 0.23 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 410S Stainless Steel, tempered at 540°C (1000°F)
410 Stainless Steel, tempered at 540°C (1000°F)
422 Stainless Steel 650°C (1200°F) temper
422 Stainless Steel 480°C (900°F) temper
422 Stainless Steel 370°C temper

MQ422AK / 13094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.