MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis Riblene® FL 20 R Film Grade Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Riblene FL 20 R is a LDPE suitable for blown film extrusion. Riblene FL 20 R is characterized by a good balance between process ability and mechanical properties. Films manufactured by Riblene FL 20 R are easily heat shrinkable and have good optical properties.

Application: Riblene FL 20 R is recommended for general packaging film, for the production of low gauge and shrink film and for blend.

Property values reported for film extruded with BUR 1:3, thickness 70 µm. Actual properties are typical and may vary depending upon operating conditions and additive package.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ISO 1183
Thickness 25.0 - 80.0 microns0.984 - 3.15 milRecommended
 70.0 microns2.76 milAs-tested; BUR 1:3
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiISO 527-3
Film Elongation at Break, MD 300 %300 %ISO 527-3
Film Elongation at Break, TD 550 %550 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50>= 0.50ISO 8295
Elmendorf Tear Strength, MD 7.10 g/micron180 g/milISO 6383-2
Elmendorf Tear Strength, TD 4.60 g/micron117 g/milISO 6383-2
Dart Drop Test 190 g0.419 lbF50; ISO 7765-1/A
Film Tensile Strength at Break, MD 25.0 MPa3630 psiISO 527-3
Film Tensile Strength at Break, TD 19.0 MPa2760 psiISO 527-3
1% Secant Modulus, MD 160 MPa23200 psiISO 527-3
1% Secant Modulus, TD 180 MPa26100 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °FManufacturer method
Vicat Softening Point 90.0 °C
@Load 1.00 kg
194 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D 746
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ISO 14782
Gloss 54 %54 %45°; ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 190 °C320 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9810 / 265688

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.