MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 El Mar® LA4 SAE 15W-40  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Hydroclear EL MAR LA4 low ash natural gas engine oil meets increasing demands for long engine life, smooth efficient operation and toughness. Made with exclusive Hydroclear technology, this gas engine oil is the one that combines the best base stock components and field-proven additives to provide outstanding engine cleanliness, wear and corrosion protection. These are all the things a gas engine needs to give dependable, efficient service with lower maintenance costs for many years. Clean engines last longer between expensive overhauls. Engine deposits that build up with lesser quality oils are abrasive to pistons, rings, valves and liners, causing shortened engine life. Hydroclear EL MAR LA4 stops deposits two ways. First, its base oil component is absent of unstable compounds which break down quickly into carbon deposits. Then, field proven additives suspend particles in the oil before they can form deposits. The result – a cleaner, more reliable and efficient engine. Hydroclear EL MAR LA4 is built to save money! Fuel is the largest operating expense for gas engines, followed by manpower and lubricant. Clean engines are able to perform at peak efficiency by allowing proper airflow and avoiding frictional losses caused by engine deposits, thus increasing fuel efficiency. Hydroclear EL MAR LA4 is recommended for use in nearly all types of turbocharged, lean burn and naturally aspirated natural gas engines requiring low ash lubricants.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.871 g/cc
Density 7.25 lb/gal
Viscosity 6000 cP
@Temperature -20.0 °C
Cold Crank
Viscosity Measurement 138Viscosity Index
Kinematic Viscosity at 40°C (104°F) 112 cSt
Kinematic Viscosity at 100°C (212°F) 15 cSt
Ash 0.50 %Sulfated Ash; ASTM D874
ASTM Color 4.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 5.5ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -38.0 °F
Flash Point 446 °FCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.028 %
Zinc, Zn 0.033 %
 
Descriptive Properties
Phosphorus260 ppm
Zinc30 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON268 / 75305

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.