GRILON M 371 is a durable siliconized fine fiber for very soft, thermobonded interlinings. The coarser counts, 3.3 - 4.8 dtex, are also used for volume nonwovens and cotton yarns. Data provided by Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |