MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexForce™ 717 Hybrid Composite Fabric
Categories: Other Engineering Material; Composite Fibers

Material Notes: Hexcel features custom fabric design and manufacturing for optimum performance. Two or more different fibers (carbon, glass, aramid, ceramics) may be combined, different weaving solutions are possible, various produce preforms, etc.

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 8.40 mil
 
Descriptive Properties
Fabric Weight (oz/yd2)5Dry
Nominal Construction (count/in)16Warp
 16Fill
Type of YarnFill Yarn: SCG 75 1/0 493
 Warp Yarn: 3K Carbon, 33 MSI
Weave StylePlain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 716 Hybrid Composite Fabric
Solvay Thornel® Mat VMC Carbon Fiber
Glassy Carbon used in heart valve prostheses
Fibre Glast 2443 Kevlar® Twill Weave Fabric
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness

PHEXC662 / 101281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.