MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dynasol Calprene® 1015 Styrene-Butadiene Rubber SBR Diblock Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Calprene 1015 is a linear high molecular weight random-block styrene/butadiene copolymer with 15% styrene, 10% present as a polystyrene block. It has a non-staining antioxidant system; FDA approved for use in food contact applications and is essentially gel free with a very clear color. Calprene 1015 is mainly used as elastomeric modifier for asphalt and as an impact modifier in polystyrene products. It is packed in bales with a low melting point polyethylene wrapping.

Information provided by Dynasol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccDIN-53479
Volatiles <= 0.75 %ASTM D-5668
Viscosity Measure 35 cStStyrene solution viscosity 5%; NM 300-11
 
Chemical PropertiesOriginal ValueComments
Styrene Content 10 %Block styrene; NM 202-07
 15 %ASTM D-5775
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Color Alpha, max15
Insolubles in toluene, 325 mesh, % max0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATG s.r.l. SBR Styrene-Butadiene Rubber
Dynasol Solprene® 303 Random-Block Copolymer
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Armacell Monarch® F-05013 (Black) Neoprene, EPDM, SBR Blend Foam
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)

PDYNA54 / 34800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.