MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CIPLAS LDD2021F Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Overview: LDD2021F is a general purpose liner resin for thin gauge applications requiring good drawdown and excellent toughness for blown and cast film extrusion.

Applications:

  • Medium Duty Produce Bags
  • Good Clarity Shrink Film
  • Bags for Textile Items
Properties:
  • Excellent Heat Sealability
  • Good Haze, Gloss, Strength and Processability
Additive:
Antiblock: 1250 ppm; Slip: 700 ppm

Information provided by CIPLAS by ITOCHU

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.9215 g/cc0.03329 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1250 ppm1250 ppm
Slip Level 700 ppm700 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.3 MPa1790 psiASTM D882
Film Tensile Strength at Yield, TD 12.1 MPa1760 psiASTM D882
Film Elongation at Break, MD 417 %417 %Ultimate; ASTM D882
Film Elongation at Break, TD 665 %665 %Ultimate; ASTM D882
2% Secant Modulus 0.18055 GPa26.187 ksiMD; ASTM D822
 0.20702 GPa30.026 ksiCD; ASTM D822
Elmendorf Tear Strength MD 498 g498 gASTM D1922
Elmendorf Tear Strength TD 284 g284 gASTM D1922
Dart Drop Test 154 g0.340 lbASTM D1709
Film Tensile Strength at Break, MD 24.80 MPa3597 psiUltimate; ASTM D882
Film Tensile Strength at Break, TD 22.95 MPa3329 psiUltimate; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °F
Vicat Softening Point 93.0 °C199 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 8.9 %8.9 %ASTM D1003
Gloss 66 %66 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 °C390 °F
Blow-up Ratio (BUR) 2.52.5
Screw Speed 60 rpm60 rpm
 
Descriptive Properties
Puncture Resistance3 J/cm3Dow Method
Toughness159 J/cm3MD, ASTM D822
 189 J/cm3CD, ASTM D822

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCIPLA004 / 283982

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.