TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus meeting specification requirements of Bellcore and connector manufacturers. This two-part, low viscosity system can be cured at room temperature overnight or as fast as 15 minutes at 65°C. Information provided by Tra-Con Inc. |