MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LCY Globalene 3542 Styrene - Butadiene block copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Features:
  • Linear and clear block copolymer
  • High strength and low viscosity
  • High tensile strength
  • High rebound
Typical Application:
  • Transparent shoe sole
  • Plastic modification
  • Asphalt modification
  • Adhesive
  • Mechanical parts

Information provided by LCY Chemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Value; ASTM D792
Volatiles 0.10 %0.10 %Value; ASTM D5668
 <= 0.50 %<= 0.50 %Range; ASTM D5668
Viscosity 1250 cP1250 cP25%/25°C Toluene, Value; ASTM D2196
 1000 - 1500 cP1000 - 1500 cP25%/25°C Toluene, Range; ASTM D2196
Melt Flow  1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Value; ASTM D1238
 1.0 - 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.0 - 3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Range; ASTM D1238
Ash 0.10 %0.10 %Value; ASTM D5667
 <= 1.0 %<= 1.0 %Range; ASTM D5667
 
Descriptive Properties
Content0.4SM Content, Value, ASTM D5775
 38-42%SM Content, Range, ASTM D5775

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLCY179 / 295722

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.