MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shanghai Potomer ZR-940(Rutile)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Characteristics: Great opacity, whiteness, lightening power, gloss, hiding power and easy dispersion, good weather resistance and chalk resistance. Designed for outdoor, exterior use

Applications: ZR-940 is the universal pigment, particularly recommended for high quality paints used for internal and external coatings, both water-borne and solvent-borne (industrial, architectural, and decorative), and printing ink. This pigment can also be successfully utilized for plastic, rubber, paper and leather, etc.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.10 g/cc
Bulk Density 0.640 g/ccnot tamped
Volatiles <= 0.80 %
@Temperature 105 °C
Particle Mesh Size 45 Mesh<0.05%
pH 6.5 - 8.0Aqueous Suspension
 
Component Elements PropertiesOriginal ValueComments
TiO2 >= 92 %
 
Descriptive Properties
Color<0.5Δsb
 >-0.3ΔL*
Oil Absorption<23 g/100g
Scattering power>100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM006 / 284452

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.