MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSRC T-BLEND® 2002-10S TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® 2002-10S is a pre-formulated and pelletized thermoplastic elastomer compound based on styrene butadiene block copolymer. Thanks to its high strength and clarity. It is designed for the injection molding of non-toxic toy components and infant product parts with improved tear and torque resistance. Being a thermoplastic elastomer, T-BLEND® 2002-10S can be easily processed with general processing equipment and tools designed for thermoplastics and yet possess elastomeric properties at ambient temperatures.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.840 - 0.900 g/cc0.840 - 0.900 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm0.0080 - 0.015 in/in
Melt Flow 35 - 75 g/10 min
@Load 2.16 kg,
Temperature 160 °C
35 - 75 g/10 min
@Load 4.76 lb,
Temperature 320 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 52 - 5852 - 58ASTM D2240
 
Processing PropertiesMetricEnglishComments
Feed Temperature 130 °C266 °F
Rear Barrel Temperature 140 °C284 °F
Front Barrel Temperature 150 °C302 °F
Die Temperature 160 °C320 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
Back Pressure 0.343 - 4.90 MPa49.7 - 711 psi
Cycle Time - Injection 35 - 50 sec35 - 50 sec
 
Descriptive Properties
ColorBlue
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC049 / 306337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.