MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical machinery, transformers and chemical plants. Suitable for mechanical applications. The flexural strength and modulus of elasticity values are measured along the sheet.

Applications: Wear parts/vanes in oil-lubricated vacuum pumps.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 EP GC 308, DIN 7735 Hgw 2372.4, NEMA LI 1 G-11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
@Temperature 23.0 °C
24h/23°C/50% RH; ISO 1183-A
Water Absorption 0.10 %ISO 62-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 320 MPa
@Thickness >=1.50 mm
24h/23°C/50% RH; ISO 527
Flexural Strength 375 MPa
@Thickness >=1.50 mm,
Temperature 180 °C
1 hour at temperature/50% RH, Normal to laminate plane; ISO 178
 500 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 24.0 GPa
@Thickness >=1.50 mm
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 600 MPa
@Thickness >=5.00 mm
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 60.0 MPa
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 80.0 kJ/m²
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 2.00e+8 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant 5.0
@Thickness <=3.00 mm,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 5.0
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
 80.0 kV/in
@Thickness >=3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
Dissipation Factor 0.0080
@Thickness <=3.00 mm,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 0.010
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 400 V
@Thickness >=3.00 mm
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
IEC 60216
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Elektro-Isola G-Etronax EP FR Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Norplex-Micarta NP130 Epoxy Glass Laminate Sheet, NEMA FR-4
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets

PELEKT048 / 126924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.