MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polypropylene (PP)

Material Notes: Recovered polypropylene and polyethylene composite

Information provided by Breplast S.p.A.

Key Words: Injection Molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.930 g/ccISO 1183-1
Melt Flow 1.5 - 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 4.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5.00 MPaISO 527
Tensile Strength, Yield 5.00 MPaISO 527
Elongation at Break 15 %ISO 527
Flexural Strength 23.0 MPaISO 178
Flexural Modulus 890 MPaISO 178
Izod Impact, Notched 9.00 J/mISO 180
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 126 °CA50; ISO 306
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2024-T3
SEKISUI SPI KYDEX® 6565 Thermoplastic
Breplast Bretene SPF M Thermoplastic Composite, 70% PP + 30% PE
Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP
AISI Type 302B Stainless Steel, annealed sheet

PBREP901 / 159346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.