MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Forplast POLYETHYLENE PEHD P 131 (PE 80) Post-Consumer Recycled HDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: PE grade code: High Density Polyethylene (Post-Consumer Recycled)

Stabilization recipe: Antacid, antioxidant thermostabilized processing aid, dispersing agent carbon black.

Application: Pipe and cable protection pipe, Extrusion, no pressure pipe.

Information provided by Forplast Srl.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 - 0.969 g/cc0.0341 - 0.0350 lb/in³Compound; ISO 1183
Carbon Black Loading 2.0 %2.0 %ASTM D1603
Melt Flow  0.15 - 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
UNI 1133T
 0.70 - 1.1 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.70 - 1.1 g/10 min
@Load 11.0 lb,
Temperature 374 °F
UNI 1133T
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 6050 - 60UNI EN ISO 868
Tensile Strength at Break >= 28.0 MPa>= 4060 psi50mm/min; UNI 5819
Tensile Strength, Yield >= 20.0 MPa>= 2900 psi50mm/min; UNI 5819
Elongation at Break >= 600 %>= 600 %50mm/min; UNI 5819
Modulus of Elasticity >= 0.700 GPa>= 102 ksiUNI EN ISO 527-2
 
Descriptive Properties
Supply formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFORP902 / 316413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.