MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 1149°C (2100°F) + Age
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Data provided by Allvac.

Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools.

Key Words: Allvac, an Allegheny Teledyne Company, UNS N07750; AMS 5667, 5668, 5669, 5670, 5671. MIL-N-24114, ASTM B 637
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 290Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 315Estimated from Rockwell C value.
Hardness, Rockwell C 30
Hardness, Vickers 304Estimated from Rockwell C value.
Tensile Strength, Ultimate 1000 MPa
Tensile Strength, Yield 655 MPa
@Strain 0.2 %
Elongation at Break 20 %
Reduction of Area 20 %
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.70 %
Carbon, C 0.040 %
Chromium, Cr 15.5 %
Iron, Fe 7.0 %
Nickel, Ni >= 70 %as balance
Niobium, Nb (Columbium, Cb) 0.95 %
Titanium, Ti 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age
Special Metals INCONEL® Alloy X-750
ATI Allvac® 520 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) + Age
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
Special Metals INCONEL® Alloy 718

NALL11 / 14779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.