MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Elastron® G SEBS Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Characteristics
  • wide hardness range
  • does not require vulcanisation-quite higher saving on the processing costs
  • remains flexible at low temperatures
  • high temperature resistance
  • electrical insulator with very low conductivity
  • has grades with very low conductivity
  • has grades with very low compression set
  • grades with very high abrasion resistance
  • excellent tear resistance
  • 100% recyclable
  • PVC free
  • resistance to solvents
  • resistance to oil
  • resistance to acids, bases, and detergents
  • resistance to UV and ozone
  • resistance to bacterial and fungus growth
  • has low toxic potential, with many grades conforming with FDA regulations
  • halogen free flame retardancy
  • coloured grades available
  • allows direct colouring during processing by utilizing coloured PP and PE masterbatches
  • 2-shot moulding onto many other plastics
  • appropriate co-extrusion process

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.890 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
Hardness, Shore D 10
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -40.0 °C
Shrinkage 1.0 - 3.5 %
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 170 - 200 °C
Middle Barrel Temperature 170 - 200 °C
Front Barrel Temperature 170 - 200 °C
Die Temperature 180 - 200 °C
Mold Temperature 30.0 - 60.0 °C
 
Descriptive Properties
Acid-Base Resistanceexcellent
Comp. Ratio2.5 - 3.5
Compression Setgood
Draw Down5-10
Dryingnot necessary
Injection Speedmedium-fast
L/D Ratio20 - 24:1
Motor Oil Resistancemedium
Solvent Resistancemedium
UV-Ozone Stabilityexcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elastron® D SEBS Elastomer
Covestro Makrolon® 2407 MAS070 Polycarbonate
Buckeye Polymers BP FLEX A6310 BLK Thermoplastic Elastomer SEBS
Elastron® TPO Elastomer
Celanese Zytel® 70G33L BK031 PA66-GF33

PELASTR01 / 80913

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.