MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silres® BS 1701 Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 1701 is a mixture of octyltriethoxysilanes isomers, with iso-octyltriethoxysilane as the main component. SILRES® BS 1701 is used in undiluted form for the hydrophobic priming and impregnation of concrete and reinforced concrete. In addition SILRES® BS 1701 is suitable for the hydrophobic treatment of fillers and pigments.

Special features: SILRES® BS 1701 is characterised by:

  • Excellent penetrating power
  • no solvents, environmentally compatible
  • low volatility
  • high resistance to alkalis
Treated concrete will have the following permanent properties:
  • dramatic reduction in chloride and water absorption
  • no loss in breathability
  • improved durability against freeze-thaw de-icing salt stress
  • enhanced durability
  • provides good adhesion for paints
In the construction material, SILRES® BS 1701 reacts with atmospheric moisture and / or the water in the building material’s pores, eliminating alcohol. The active thus substance formed greatly reduces the concrete’s absorbency in the active zone (penetration depth after post treatment), but without blocking any pores or capillaries. The impregnated building material retains very high water-vapor permeability.

Application: SILRES® BS 1701 is recommended for the hydrophobic impregnation and priming of concrete and reinforced concrete in road, bridge and building construction. In addition it is suitable for the hydrophobic treatment of fillers and pigments.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³DIN 51757
Viscosity 1.9 cP1.9 cPdynamic; DIN 51562
Molecular Weight 276 g/mol276 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point 236 °C
@Pressure 0.1013 MPa
457 °F
@Pressure 14.69 psi
Flash Point >= 40.0 °C>= 104 °FISO 3679
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear colorless
Content (%)99Silane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9553 / 205082

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.