MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostacom BFT 30 Polypropylene with 30% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Hostacom BFT 30 is a 30% talc filled PP copolymer, with good stiffness. The product is available in black color, pellet form. Applications: Automotive Parts

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1A
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 2400 MPaTech.A; ISO 178/A1
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom 68F4-3 BLK Polypropylene with 30% Talc Filler
LyondellBasell Hostacom EKC 455P G82779 Polypropylene with 30% Talc Filler
LyondellBasell Astryn 65F4-3 Polypropylene Homopolymer, 30% Talc
LyondellBasell Hifax ERC 347P G14008 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom EKC 425N G91428 Polypropylene Elastomer Modified Talc Filled

PEQT7677 / 219314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.