Hostacom DYS707N NATRL high melt flow, 1050 MPa flexural modulus, high impact, natural thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, impact resistance and processability. It is typically used for automotive interior trim applications that demand balanced performance characteristics. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |