MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
GLS Corporation Versaflex™ HC 2110-54B Healthcare Gasket and Stopper Grade TPE, Low Stiction  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Versaflex™ products meet the requirements and end-use environments in the healthcare, consumer, electrical and electronics, packaging and appliance markets. This family of thermoplastic elastomers utilizes the available thermoplastic elastomer technologies to create compounds and alloys with highly specialized characteristics. Featured characteristics of Versaflex™ TPEs include:

  • Adhesion to a range of engineering plastics
  • Clear, heat resistant TPEs
  • Excellent colorability
  • Ultra-clear grades
  • Ultra-soft TPEs down to 30 Shore OO
  • FDA, USP VI, ISO 10933 approved grades
  • NSF, and UL 94 listed grades
  • Extrusion, injection, and blow moldable
  • Sterilizable under autoclave, radiation and EtO gas

All information provided by GLS Corporation. GLS Corporation and PolyOne (now Avient) merged in 2008. This discontinued grade was produced by GLS Corporation and is in MatWeb with the GLS name for historical accuracy.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792 / ISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5410 second delay; ASTM D2240 / ISO 868
Tensile Strength at Break 645 psiASTM D 412-Die C
Elongation at Break 190 %ASTM D 412-Die C / ISO 37
Compression Set 15 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM 395B
 
Compliance PropertiesOriginal ValueComments
FDA Yes
USP Class VI Yes
 
Descriptive Properties
2002/72/ECYes
EtO SterilizationYes
ISO 10933Yes
PP BondableYes
Radiation SterilizationYes
RoHSYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZGLSCC837 / 92897

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.