MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Raschig Group DECAL® 152CL Phenolic
Categories: Polymer; Thermoset; Phenolic

Material Notes: Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS)

Processing: Injection and compression molding

Applications: Parts under mechanical and temperature loading

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 - 1.80 g/ccISO 1183
Apparent Bulk Density 0.600 - 0.800 g/ccISO 60
Water Absorption <= 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmInjection and Compression; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.0 - 90.0 MPaCompression; ISO 527
 90.0 - 110 MPaInjection; ISO 527
Modulus of Elasticity 6.00 - 9.00 GPaInjection and Compression; ISO 527
Flexural Strength 110 - 140 MPaCompression; ISO 178
 150 - 180 MPaInjection; ISO 178
Flexural Modulus 11.0 - 13.0 GPaCompression; ISO 178
 12.0 - 14.0 GPaInjection; ISO 178
Compressive Strength 250 - 300 MPaISO 604
Charpy Impact Unnotched 7.00 - 10.0 kJ/m²Compression; ISO 179/1eU
 13.0 - 17.0 kJ/m²Injection; ISO 179/1eU
Charpy Impact, Notched 2.00 - 4.00 kJ/m²Compression; ISO 179/1eA
 3.00 - 5.00 kJ/m²Injection; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 - 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohmIEC 60093
Dielectric Constant 4.0 - 6.0
@Frequency 1e+6 Hz
IEC 60250
 6.0 - 8.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 - 30.0 kV/mmIEC 60243-1
Dissipation Factor 0.010 - 0.020
@Frequency 100 Hz
IEC 60250
 0.020 - 0.030
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 180 - 240 secASTM D495
Comparative Tracking Index >= 225 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 - 16.0 µm/m-°C
@Temperature 50.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.400 - 0.600 W/m-KASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-A
Deflection Temperature at 8.0 MPa >= 170 °CISO 75-C
Flammability, UL94 V-0
@Thickness 1.50 mm
Shrinkage <= 0.20 %
@Temperature 110 °C,
Time 605000 sec
Post shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 20.0 - 30.0 °C
 
Descriptive Properties
Glow wire flammability test960/1IEC 60695 2-12
Glow wire ignitability test960/1IEC 60695 2-13
Water Absorption<20 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit 4421 XB Novolac Phenolic
Raschig Group DECAL® 937 Phenolic
Plenco 5118 Phenolic, Granular, Compression Molded
Plenco 4300 Phenolic, Granular, Compression Molded
Overview of materials for Phenolic; Unreinforced; Molded

PRASCI20 / 179157

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.