MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum 2011-T8
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Information provided by Alcoa and the references. General 2011 characteristics and uses: Good machinability, especially free-cutting qualities, good mechanical properties. Excellent surface finish capability. The T451 temper offers good deep drilling characteristics.

Uses: Adapters, carburetor parts, clock parts and gears, knobs, camera parts, meter shafts and gears, nozzles, pencil and pen parts, oil line filters, pipe stems and filters, radio parts, screwdriver caps, spindles, telephone parts, TV fittings, tripod fittings, machine parts, hose parts, pipe stems.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2011-T8; UNS A92011; QQ-A-225/3; NF A-U4Pb (France); DIN AlCuBiPb; BS FC1; AA2011-T8; Al2011-T8
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.83 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 100AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 126Converted from Brinell Hardness Value
Hardness, Rockwell A 41.4Converted from Brinell Hardness Value
Hardness, Rockwell B 63Converted from Brinell Hardness Value
Hardness, Vickers 112Converted from Brinell Hardness Value
Tensile Strength, Ultimate 59.0 ksiAA; Typical
 >= 370 MPa
@Thickness 3.17 - 82.5 mm
Rolled or cold finished wire, rod, and bar
Tensile Strength, Yield 45.0 ksiAA; Typical
 >= 275 MPa
@Thickness 3.17 - 82.5 mm
Rolled or cold finished wire, rod, and bar
Elongation at Break >= 10 %
@Thickness 3.17 - 82.5 mm
Rolled or cold finished wire, rod, and bar
 12 %
@Diameter 12.7 mm
AA; Typical
Modulus of Elasticity 10200 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.33
Fatigue Strength 18000 psi
@# of Cycles 5.00e+8
completely reversed stress; RR Moore machine/specimen
Machinability 90 %0-100 Scale of Aluminum Alloys
Shear Modulus 26.0 GPa
Shear Strength 35.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 23.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.7 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.4 µm/m-°C
@Temperature -50.0 - 20.0 °C
 24.0 µm/m-°C
@Temperature 20.0 - 200 °C
 25.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Thermal Conductivity 1190 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 1005 - 1190 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting can be eliminated by homogenization.
Solidus 1005 °FAA; Typical
Liquidus 1190 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 775 °F
Solution Temperature 975 °F
Aging Temperature 320 °F14 hr at temperature
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 91.2 - 94.6 %As remainder
Bismuth, Bi 0.20 - 0.60 %
Copper, Cu 5.0 - 6.0 %
Iron, Fe <= 0.70 %
Lead, Pb 0.20 - 0.60 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.40 %
Zinc, Zn <= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2011-T3
Aluminum 2011-T6
Aluminum 2011-T4
Aluminum 2007-T3
Aluminum 2024-T6

MA2011T8 / 8836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.