MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Features

Modified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Linear Mold Shrinkage 0.0175 cm/cm
Linear Mold Shrinkage, Transverse 0.0182 cm/cm
Melt Flow 25 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.0 MPa
Elongation at Break 5.0 %
Tensile Modulus 3200 MPa
Flexural Strength 88.0 MPa
Flexural Modulus 3150 MPa
Charpy Impact Unnotched 11.0 kJ/m²
@Temperature -20.0 °C
 25.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 1.00 kJ/m²
@Temperature -20.0 °C
 2.00 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
Vicat Softening Point 142 °CB
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 40.0 - 50.0 °C
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling
Plastcom SLOVALEN PC 93 T 30 PP reinforced with 30% mineral filler
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling

PPLACO281 / 120905

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.