MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Tuflin™ HS-7001 NT 7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: Tuflin™ HS-7001 NT 7 LLDPE is an antioxidant modified ethylene-hexene-1 copolymer resin designed for slot cast extrusion. It is supplied in pelleted form. Films produced fro HS-7001 NT 7 exhibit high clarity, high tensile strength, high elongation and good puncture resistance. This resin has outstanding drawdown capability.
Main Characteristics:
  • Designed for slot cast thin film applications including stretch and clip wraps
  • High clarity
  • Superior toughness
  • Compiles with US FDA 21 CFR 177.1520©3.1a
Availability: North America

Agency Ratings: FDA 21 CFR 177.1330(a)

Additive: Antiblock: No; Processing Aid: No; Slip: No

Form: Pellets

Processing Method: Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D792
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 750 %
@Thickness 0.0254 mm
ASTM D882
Film Elongation at Break, TD 830 %
@Thickness 0.0254 mm
ASTM D882
1% Secant Modulus 24000 psi
@Thickness 0.0254 mm
MD; ASTM D882
 25000 psi
@Thickness 0.0254 mm
TD; ASTM D882
Elmendorf Tear Strength MD 370 g
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength TD 500 g
@Thickness 0.0254 mm
ASTM D1922
Dart Drop Test 120 g
@Thickness 0.0254 mm
ASTM D1709A
Film Tensile Strength at Break, MD 4700 psi
@Thickness 0.0254 mm
ASTM D882
Film Tensile Strength at Break, TD 4200 psi
@Thickness 0.0254 mm
ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 2.5 %
@Thickness 0.0254 mm
ASTM D1003
Gloss 90 %
@Thickness 0.0254 mm
45°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 510 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF565 / 311258

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.