MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell AP Armaflex® SA Through 1" Duct Liner and Wrap
Categories: Other Engineering Material

Material Notes: The original, fiber-free, closed-cell thermal and acoustical duct insulation – with a laborsaving pressure sensitive system – engineered to safeguard IAQ, attenuate HVAC noise and reduce energy waste. AP Armaflex FS SA is PVC free.
  • Fiber-free, non-particulating, formaldehyde-free, free of PDBE flame retardants, and low VOC
  • Attenuates airborne noise to reduce background noise from HVAC systems
  • Meets ASHRAE 90.1 - 2010, ASHRAE Standard 189.1,
  • IECC 2012 and California Title 24 for increased energy efficiency
  • Designed to last the useful life of mechanical equipment
  • Pressure sensitive adhesive system saves installation labor costs
  • Microban® antimicrobial product protection inhibits the growth of mold and mildew in the insulation

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.20 %ASTM C209
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0353 W/m-K
@Temperature 24.0 °C
ASTM C177 or C518
 0.0366 W/m-K
@Temperature 32.0 °C
ASTM C177 or C518
Insulation R Value 1.60
@Thickness 9.52 mm
 2.10
@Thickness 12.7 mm
 3.10
@Thickness 19.0 mm
 4.20
@Thickness 25.4 mm
 6.00
@Thickness 38.1 mm
 8.00
@Thickness 50.8 mm
Maximum Service Temperature, Air 82.0 °CASTM C534
Minimum Service Temperature, Air -183 °CASTM C534
Flame Spread Index 25ASTM E84
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Smoke Developed Index50ASTM E84
Water Vapor Permeability0.05 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARMD006 / 186617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.