MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D1193 P (SIS) Linear Triblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1193 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 24%. It is supplied from North America in the physical form identified:
Kraton D1193 PT - supplied as a dusted dense pellet

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1193 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccASTM D4025
Volatiles <= 0.30 %KM 04
Viscosity 400 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Ash 0.15 - 0.35 %Talc; BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
@Time 10.0 sec
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 17.9 MPaTypical properties determined of film cast from toluene solution; ASTM D412
Elongation at Break 1200 %Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.00255 GPa
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentAntioxidant0.08-0.3%, KM 08
 Polystyrene22.7-25.7%, KM 03
 Total Extractables<1.2%, KM 05
Styrene/Rubber Ratio24/76

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer
Kraton® D1160 E (SIS) Linear Triblock Copolymer
Kraton® D1161 J (SIS) Linear Triblock Copolymer

PKRA9880 / 132779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.