MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Shanghai Potomer YS-770(HALS) Hindered Amine Light Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS NO. 52829-07-9

Characteristics and Uses: YS-770 is a hindered amine light stabilizer (HALS) for applications demanding particularly high light stability. It is recommended to be used in PP, EPDM, PS, HIPS, ABS, SAN, ASA and PUR and is also effective in PA and polyacetals. It is provides excellent light stability for thick sections and films in the recommended substrates. Benefits of using YS 770 is the high light-stabilizing performance, particularly in PP thick sections. It has broad compatibility and can be easily dispersed. Compared to conventional UV-absorbers, the effectiveness of YS 770 is less dependent on the polymer’s thickness. For this reason the use of YS 770 also provides good light stability in articles with higher specific surface, e.g. films and tapes. The recommended concentrations range between 0.1% and 0.5%, depending on the substrate, processing conditions and application.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
pH >= 9.67>= 9.671% suspension in water 20-25°C
Vapor Pressure 0.00134 bar1.00 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 - 86.0 °C176 - 187 °F
Flash Point >= 150 °C>= 302 °F
Ignition Temperature 330 °C626 °F
 
Descriptive Properties
Color/AppearanceWhite crystalline powder or granules
Partition coefficient0.35Log Pow, 20-25°C
Solubility1 mg/LWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM111 / 284557

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.