MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products BC-709 Urethane Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: BC-709 is a two-component urethane system consisting of Part A & Part B. It is designed to be used where a high level of mechanical properties of cured material is desired when curing at ambient temperatures.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccPart A
 0.939 g/ccPart B
Viscosity 1250 - 1450 cPPart B
 3600 - 4200 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73 - 77
Tensile Strength, Ultimate 950 - 1250 psi
Elongation at Break 325 - 475 %
Resilience 35 - 40Bayshore
Tear Strength 30.0 - 40.0 plisplit
 160 - 200 pliDie C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourDemold time
 168 hourCuring time for max properties
Pot Life 30.0 - 40.0 min50,000 cps
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorless to yellow liquidPart A
 Yellow to amber liquidPart B
Mix ratio100:45Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC100 / 250965

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.