MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Rykon® ISO 68 Premium Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.

They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion inhibitors, foam and aeration suppressants, and a shear stable viscosity index improver.

Hydraulic systems, due to the nature of their operation, experience accelerated wear unless they are protected by clean, high quality antiwear hydraulic oils. Surging pressures in pumps and valves can increase metal-to-metal contact unless antiwear protection is present. The antiwear additives in Chevron Rykon Premium Oils plate out on the metal surfaces. This plating minimizes metal-to-metal contact, which is most severe in vane-, piston-, and gear-type pumps. As hydraulic pressures increase over 1000 psi, the need for antiwear protection increases proportionally.

Applications

Chevron Rykon Premium Oils are versatile lubricants available in multiviscosity ISO 15, 22, 32, 46, 68, and 100.

The multiviscosity feature allows even and continuous power transmission over a wide temperature range with a minimum of shudder, and increased accuracy. They are recommended for hydraulic or circulating oil systems, including marine on-deck machinery, hydraulic actuated loading bins, or equipment which runs at various operating temperatures.

Chevron Rykon Premium Oils ISO 32, 46, and 68 meet all major pump manufacturers requirements including:

  • Vickers I-286-S, M 2950-S, 35VQ 25
  • Racine Model S
  • Cincinnati Machine P 68 (ISO 32), P 70 (ISO 46), P 69 (ISO 68)
  • Denison HF-0, HF-2

In a clean, dry environment, Chevron Rykon Premium Oils ISO 15, 22, 32, 46, 68, and 100 typically meet a dielectric strength of 35 kV (ASTM D 877).

Chevron Rykon Premium Oils meet the requirements (discontinued in 1998) of the U.S. Department of Agriculture (USDA) for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.

Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Key Words: CPS Number: 232952; MSDS Number: 7341
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.1 °
Viscosity Measurement 154Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 346 SUS
Saybolt Viscosity at 210°F 63.8 SUS
Kinematic Viscosity at 40°C (104°F) 68 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11 cStASTM D445
Oxidative Stability >= 6000 hourHours to 2.0 mg KOH/g acid number; ASTM D943
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/in
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °CASTM D97
Flash Point 212 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Rykon® ISO 68 Oil AW
ChevronTexaco Rykon® ISO 32 Premium Oil

WCHEV354 / 74969

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.