MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes:

Information provided by Eurotec®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
0.200 %
@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inEurotec
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inEurotec
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 9.00 GPa1310 ksiISO 527
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Comparative Tracking Index 175 V175 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °FISO 75
Vicat Softening Point 145 °C
@Load 5.10 kg
293 °F
@Load 11.2 lb
ISO 306
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Ignition Temperature 925 °C
@Thickness 2.00 mm
1700 °F
@Thickness 0.0787 in
IEC 60695
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 310 °C518 - 590 °F
Feed Temperature 60.0 - 80.0 °C140 - 176 °FThroat
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 120 °C248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %ISO 960
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
 
Descriptive Properties
Back PressureLow
Injection SpeedMedium - Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black
LNP Lexan® LF1010N Polycarbonate, 10% Glass Fiber Reinforced, 10% PTFE Lubricant
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Envalior Pocan® A 3131 000000 PBT+PC, 30% Glass Fiber Reinforced
Covestro Bayblend® FR3021 GR PC/ABS Blend, 15/30% Mineral/Post Consumer recycled Reinforced

PEUROS162 / 147152

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.