MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Abhar Polymer Compounds APINS01 Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APINS01 is a high density polyethylene compound suitable for insulation. The PABHAR is stabilized against thermal and shear degradation, it has excellent long term properties and demonstrates excellent extrusion ability.

Specification: ASTM D1248 / type III ,class A, category 4,grade E8,E9

Information provided by Abhar Polymer Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 - 0.960 g/cc0.0340 - 0.0347 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
ESCR 10% Igepal® >= 2000 hour
@Temperature 50.0 °C
>= 2000 hour
@Temperature 122 °F
ASTM D1693
Oxidative Induction Time (OIT) >= 30 min
@Temperature 200 °C
>= 30 min
@Temperature 392 °F
ASTM D3895
Melt Flow <= 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 0.35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57 - 61
@Time 15.0 sec
57 - 61
@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 25.0 MPa>= 3630 psiASTM D638/IEC 60811-1-1
Elongation at Break 500 - 900 %500 - 900 %10 days at 110°C; ASTM D638/IEC 60811-1-1
 >= 900 %>= 900 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC60093
Dielectric Strength 10.0 kV/mm
@Thickness 2.00 mm
254 kV/in
@Thickness 0.0787 in
No breakdown; EC60243
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 115 °C>= 239 °FISO 306
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 180 °C320 - 356 °F
Zone 2 170 - 190 °C338 - 374 °F
Zone 3 180 - 200 °C356 - 392 °F
Zone 4 190 - 210 °C374 - 410 °F
Die Temperature 240 - 260 °C464 - 500 °F
Head Temperature 210 - 230 °C410 - 446 °F
Drying Temperature <= 90.0 °C<= 194 °F
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PABHAR005 / 249438

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.