MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 10S Welding flux
Categories: Ceramic

Material Notes: Sandvik 10S is a slightly chromium compensating agglomerated flux giving good slag removal and fine bead appearance. It is primarily used for submerged arc welding with strip electrodes of the chromium, chromium and chromium nickel molybdenum types with or without niobium. This flux can also be used for wire electrodes. Sandvik 10S is an all round flux which can be used for many applications including joining stainless steels where controlled ferrite is required and surfacing large vessels with strip electrodes in petrochemical plants. Sandvik 10S gives about 2% lower ferrite content than flux Sandvik 10SW.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.00 g/cc
 
Component Elements PropertiesOriginal ValueComments
Al2O3 15 %
Chromium, Cr 2.0 %
MgO 30 %
SiO2 35 %
 
Descriptive Properties
CaF27%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5059 / 199623

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.