MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

USI Corporation EVATHENE® UE633 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Description: EVATHENE® UE633 is an ethylene-vinyl acetate copolymer resin (EVA) for use in injection molding and extrusion coating machine.

Characteristics:

  • Flexibility
  • Elasticity
  • Excellent adhesion
  • Good low temperature resistance
  • Good resistance to environmental stress cracking
  • Non-toxicity
Main Application:
  • Hot melt adhesives
  • Extrusion coating

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D792
Vinyl Acetate Content 19 %19 %USI
Melt Flow 20 g/10 min20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888ASTM D2240
Tensile Strength at Break 12.7 MPa1840 psiMolded; ASTM D638
Elongation, Ultimate 790 %790 %Molded; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 83.0 °C181 °FASTM D3418
Vicat Softening Point 60.0 °C140 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSIC011 / 285379

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.