MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elmet-Starck Molybdenum Alloy TZM AFBT, Arc-Cast Forging Billet
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought forging billets produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting process.

Structure: The billets will be supplied in the recrystallized condition, with a maximum hardness of 215 B.H.N. (10 mm ball/1500 kg/30 sec.). Material can also be supplied in the stress-relieved condition.

Information provided by H.C. Starck.

Elmet Technologies Acquired H.C. Starck Solutions Americas in 2023.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 215
@Load 1500 kg,
Time 30.0 sec
<= 215
@Load 3310 lb,
Time 0.00833 hour
10 mm ball
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 - 0.030 %0.010 - 0.030 %
Iron, Fe <= 0.0080 %<= 0.0080 %
Molybdenum, Mo >= 99.25 %>= 99.25 %by difference
Nickel, Ni <= 0.0020 %<= 0.0020 %
Nitrogen, N <= 0.0020 %<= 0.0020 %
Oxygen, O <= 0.0025 %<= 0.0025 %
Silicon, Si <= 0.0080 %<= 0.0080 %
Titanium, Ti 0.40 - 0.55 %0.40 - 0.55 %
Zirconium, Zr 0.060 - 0.12 %0.060 - 0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elmet-Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar
P/M Molybdenum TZM (Mo-0.5Ti-0.1Zr; Mo Alloy 364), Stress Relieved
Arc Cast Molybdenum TZM (Mo-0.5Ti-0.1Zr; Mo alloy 363), Stress Relieved
Arc Cast Molybdenum TZM (Mo-0.5Ti-0.1Zr; Mo Alloy 363), Recrystallized
Goodfellow TZM Molybdenum High Temperature Alloy

NHCST918 / 130808

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.