MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NextGen Adhesives P907-10 Optical Assembly Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: NGAC P907-10 is a low viscosity and optically clear adhesive system that is specifically formulated for bonding and potting applications involving optical components and assemblies.

Advantages and Applications: Uses include laminating, bonding and sealing applications requiring superior wetting, high impact strength and optically clear properties. The NGAC P907-10 is easily mixed and cured at room temperature and provides excellent adhesion to glass/glass fibers, ceramics, metals and plastic.

Information Provided by Nextgen Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Solids Content 100 %
Viscosity 200 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -60.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55
 
Processing PropertiesOriginal ValueComments
Cure Time 120 - 240 min
@Temperature 65.0 °C
 1440 min
@Temperature 25.0 °C
Pot Life 120 min
 
Descriptive Properties
ColorClear
Mix Ratio by Weight (R/H)100/30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
Resin Technology Group TIGA 110-EXDP Low Viscosity, Optically Clear Glass Bonder
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
Kolon CY312 Silicone Release Film

PNEXT006 / 90253

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.