INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form. INNOPOL® CS 2-7120 is recommended for extrusion of sheets and profiles, where the required properties are the balanced stiffness and impact resistance. Information provided by INNO-COMP |