MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALTECH® PA66 B 1000/109 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Base Polymer: Polyamide 66

Special Features: Heat ageing stabilization, easy release (demolding)

Market Segment: Various

Application Area: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 2.8 %Humidity; Sim to ISO 62
 8.5 %Sim to ISO 62
Viscosity Test 145 cm³/g96% H2SO4 5 g/l; ISO 307
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.013 cm/cm
@Time 86400 sec
ISO 294-4
Storage Temperature <= 30.0 °Cdry, protected from light
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPaISO 527
Elongation at Break 15 %ISO 527
Tensile Modulus 3200 MPaISO 527
Flexural Strength 120 MPaISO 178
Flexural Modulus 2900 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 5.50 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+12 ohmDIN EN 62631-3-2
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 264 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75-1/-2
Vicat Softening Point 242 °CB50; ISO 306
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °CInjection molding
Mold Temperature 40.0 - 80.0 °CInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 13G50 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 13005 Polyamide 66, General Purpose
Arkema Orgalloy® RS 6630 BLACK Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Arkema Orgalloy® RS 6620 NAT Polyamide 6.6 Alloy 20% Glass Fiber reinforced
Arkema Orgalloy® RS 6600 BLACK Polyamide 6.6 Alloy

PALBIS8754 / 242813

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.