MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Evonik CYROLITE® Protect Acrylic-polycarbonate alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic/Polycarbonate Alloy

Material Notes: CYROLITE® Protect and CYROLITE® Protect 2 acrylic-based multipolymer compounds and CYREX® Protect acrylic-polycarbonate alloy provide antimicrobial capabilities against a variety of microorganisms commonly found in healthcare facilities. Antimicrobial products are used in medical devices for secondary infection management or to inhibit bacterial growth.

Benefits:

  • Antimicrobial capabilities within the polymer structure. No secondary operations required.
  • Chemical resistance to lipids and alcohol
  • Easily welded
  • Bondable to PVC tubing
  • Excellent impact strength
  • EtO, gamma and e-beam sterilizable
Transparent green tint, easy to process and free of bisphenol A (BPA)

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.3 MPaASTM D638
Elongation at Break 17 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Tensile Modulus 1800 MPaASTM D638
Flexural Strength 61.0 MPaASTM D790
Flexural Modulus 1.90 GPaASTM D790
Izod Impact, Notched (ISO) 1.70 kJ/m²
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
Vicat Softening Point 94.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 32 %
@Thickness 1.50 mm
ASTM D1003
Transmission, Visible 11 %
@Thickness 1.50 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 238 - 254 °C
Mold Temperature 60.0 - 77.0 °C
Drying Temperature 71.0 °CPredrying
Dry Time 3.00 - 4.00 hourPredrying

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy
Röhm CYROLITE Med2 Acrylic-Based Multipolymer Compound
Röhm CYROLITE® Protect 2 Acrylic-polycarbonate alloy
Evonik CYREX® Protect Acrylic-polycarbonate alloy
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant

PEVONIL073 / 196277

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.