MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cookson Group STAYCHIP® 2078E No-Flow Fluxing Underfill  (discontinued **)
Categories: Polymer; Adhesive; Thermoset

Material Notes: STAYCHIP 2078E no-flow underfill is used to perform the dual functions of a solder flux and an underfill between (1) a flip chip die and a substrate or (2) an area array device and a printed circuit board. This material functions as a flux as it solders Sn63/Pb37 bumped pads to common pad metallizations (eutectic Sn/Pb, Cu/Ni/Ag, and OSP coated Cu), using a conventional reflow profile. The product also functions as an underfill as it cures during the conventional reflow profile, immediately after soldering, forming a stress absorbing, compliant matrix that distributes the stress imposed by the CTE mismatch between the die and substrate. This matrix provides enhanced environmental protection and shock resistance.

Features:

  • Uses conventional reflow profile to fully cure, with no post-reflow cure needed
  • Little or no voiding when the appropriate STAYCHIP no-flow underfill product is matched to the desired reflow profile
  • Excellent wetting
  • Cure kinetics matched to common Sn63 reflow profiles for high yield process
  • Very low ionic content
  • Exceptional thermal shock/impact resistance

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/cc
Moisture Absorption at Equilibrium 0.855 %2 hour boil; ASTM D 570-98
Viscosity 500 - 1500 cP
@Temperature 25.0 °C
Storage Temperature <= -40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D 2240
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.129
@Frequency 100000 Hz
 2.658
@Frequency 1000 Hz
 2.864
@Frequency 1e+6 Hz
 2.971
@Frequency 10000 Hz
Dissipation Factor 0.0025
@Frequency 10000 Hz
 0.0054
@Frequency 1e+6 Hz
 0.0066
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°C
@Temperature 20.0 °C
Alpha 1
 222 µm/m-°C
@Temperature 20.0 °C
Alpha 2
Glass Transition Temp, Tg 130 °CASTM D3418-82
 
Processing PropertiesOriginal ValueComments
Pot Life 1440 min
@Temperature 25.0 °C
Shelf Life 6.00 Month
@Temperature -40.0 °C
 
Descriptive Properties
AppearanceAmber
Chemical TypeEpoxy
Ionic Content, Acetate1.8 ppm
Ionic Content, Ca.55 ppm
Ionic Content, Cl0.1 ppm
Ionic Content, K.015 ppm
Ionic Content, Na0.6 ppm
Ionic Content, Nitrate0.1 ppm
Storage Modulus1.8 GPaASTM D570-98

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver-Magnesium-Nickel Alloy Strip (Ag-0.25Ni-0.25Mg), Soft Temper

PPLASK083 / 56373

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.