MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Features

PA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can be changed by the ideal combination of the glass fibre and the glass beads. High surface brightness, low rolling resistance force. Manufacturing of exact parts /mainly in flat form/, throttle valves in air piping. Increased strength and tension modulus in tension due to the addition of glass fibre. Delivered in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/cc
Viscosity Measurement 0.42 - 0.53
Linear Mold Shrinkage 0.0042 cm/cm
Linear Mold Shrinkage, Transverse 0.0053 cm/cm
Melt Flow 1.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 125 MPa
Elongation at Break 3.0 %
Tensile Modulus 7350 MPa
Flexural Strength 225 MPa
Flexural Modulus 5800 MPa
Charpy Impact Unnotched 32.0 kJ/m²
@Temperature -20.0 °C
 35.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
 4.00 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Strength 85.0 kV/mm
Comparative Tracking Index 500 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 242 °C
Vicat Softening Point 251 °CB
Flammability, UL94 HB
Glow Wire Test 650 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 70.0 - 80.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre
Domo TECHNYL® 2417IG PA66, 20% glass fiber, DRY
BASF Ultramid® A3WG8 BK 20560 40% Glass Filled PA66 (Dry)
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Conditioned)
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)

PPLACO437 / 121061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.