MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Yuyao Zhonga G30S PET, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Reinforced, flame retardant PET offers good mechanical properties, good fatigue resistance, thermo-oxidizing resistance, soldering resistance, good dielectric strength, good flow and processability; good flammability after joined flame retardant agent. Reinforced, flame retardant PET is used for household electric appliance parts, communications, equipments, printed plate board, rectifier parts, industrial switchboard, electrical appliances with inlays, electric coil skeleton, integrated circuit parts, automobile electrical appliances, etc.

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 175 MPaASTM D638
Elongation at Break 1.7 %ASTM D638
Flexural Strength 240 MPaASTM D790
Flexural Modulus 9800 MPaASTM D790
Charpy Impact, Notched 9.70 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 247 °CASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 285 °CInjection Temp
Mold Temperature 60.0 - 100 °C
Drying Temperature 125 - 130 °C
Dry Time 5.00 - 8.00 hour
Injection Pressure 80.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PYUYZ058 / 281851

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.