MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions SF M7120 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ASTM D2240
Tensile Strength, Yield 47.6 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 13 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2530 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 80.7 MPaASTM D790
Flexural Modulus 2920 MPaASTM D790
Izod Impact, Notched 640 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 61.1 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 67.8 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.6 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 63.3 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Descriptive Properties
FeaturesHigh Flow
 High Impact Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesDecorative Parts
 General Purpose
 Outdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Karina 822-18/599-CRB-LMP Gray PVC Compound
Karina 805-10/152-A-ERYB White PVC Compound
Karina 837-10/119-E-ERYB White PVC Compound
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound

PH0POL1277 / 145846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.