MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil MED-4960 Liquid Silicone Rubber - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high consistency rubbers (HCRs). They are typically supplied as two-component systems and formulated in a 1:1 mix ratio. Because their consistency is akin to petroleum jelly, they are often pumped with injection molding equipment to form molded components such as o-rings, gaskets, valves, seals, and other precision molded parts.

LSRs are designed for liquid injection molding (LIM) processes which may utilize single or multi-cavity molds, or for overmolding processes. Originally designed for automated systems, they are developed with high volume applications in mind and benefit from their high strength. Features of liquid silicone rubbers include the following:

  • Ideal for high throughput manufacturing
  • Platinum cure system—no post cure required
  • Typical work time in excess of 72 hours
  • Cure rapidly at elevated temperatures
  • Easily pigmented using NuSil color masterbatches
Comments: Injection Molding Elastomer

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60Typical
 55 - 65Certified
Tensile Strength at Break 7.60 MPaCertified
 9.00 MPaTypical
Tensile Stress at Strain 600 psi
@Strain 200 %
Elongation at Break 400 %Certified
 525 %Typical
Tear Strength 230 pliCertified
 260 pliTypical
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 35.0 g/min
Cure Time <= 5.00 min
@Temperature 165 °C
Working Life 24.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-4065 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
NuSil MED-4055 Silicone Ultra High Performance High Consistency Elastomer - Restricted Medical Use
NuSil R-1082 Silicone Engineering Coating

PNUSIL390 / 142114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.