MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech UltraTuf SG Polycarbonate Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Description: Polycarbonate Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 9360 psiASTM D638
Tensile Modulus 350000 psiASTM D638
Flexural Yield Strength 13500 psiASTM D790
Flexural Modulus 340000 psiASTM D790
Izod Impact, Unnotched 17.0 ft-lb/inASTM D256
Falling Dart Impact 960 ft-lb73°F, No Break; ASTM D3029
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 270 °FASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 90 %Gardner; ASTM D2523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NUDEC® PC Polycarbonate Sheet
Evonik Cyrolon® AR Polycarbonate Sheet
Spartech UltraTuf SP-7010 Polycarbonate Sheet
Ethylene Propylene Rubber (EPM, EPDM)
Röhm Acrylite® GMS Acrylic Sheet, Aerospace Grade

PSPAR083 / 68524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.