MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyrocks Chemical 5000A Polypropylene, halogen-free flame retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: 5000(+)is halogen-free flame retardant polypropylene with phosphorus and nitrogen as the flame retardant elements. Carbonize and expansion mechanism play the flame retardant performance. The flammability can reach UL94-V0 (0.75mm?1.5mm and 3.0mm),and passed 70?×168 hours water immersion test(UL746C), glow-wire test meets GWIT750? and GWFI960??5000(+) has the characteristics of low density of finished products, low smoke, less corrosion to the mould etc. 5000(+)halogen free flame retardant PP have UL certification, and meet the requirements of RoHS?SVHC?PFOS & PFOA?16P?Halogen-free?PAHs...etc.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 - 1.10 g/cc0.0383 - 0.0397 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm0.012 - 0.014 in/inASTM D955-08
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.0 MPa3190 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Flexural Strength 36.0 MPa5220 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FASTM D-648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
after 70°C×168h water immersion test
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
after 70°C×168h water immersion test
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
after 70°C×168h water immersion test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROCKS000 / 278508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.