Notes: Monprene OM-16175 is a specialty thermoplastic elastomer designed for overmolding applications like grips and anti-skid parts for a variety of consumer and industrial products. Monprene OM-16175 is a medium hardness, low density, opaque grade that is available in Black, Natural, and can be pre-colored, and exhibits excellent adhesion to nylon. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Bondability; Good Adhesion; Good Colorability; Light Stabilized; Lubricated; Medium Flow; Medium Density; Medium Hardness; Lubricated; Slip Uses: Bonding; Cell Phones; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Rubber Replacement; Sporting Goods RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |