MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASI® Pipe Sealer TORQUE 171 Anaerobic Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TORQUE 171 is a Anaerobic adhesive for sealing of metal thread pipe joints. Replaces PTFE tape and yarn, gives instant sealing against moderate pressure, gives elastic cured film. Low friction coefficient will assure easy assembly. Thixotropic property prevents migration from thread of the sealant before or during curing. Shocks and vibrations resistances are unaffected properties of sealing in the range of temperature from -55 to +150°C. Easy dismantling is assured even after years.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccuncured
Viscosity 4000 cP
@Temperature 25.0 °C
uncured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 435 - 725 psiZinc plated bolt M 10x20- quality 8.8- nut h=0.8d.; ASTM D2095
Shear Strength 580 - 870 psiZinc plated bolt M 10x20- quality 8.8- nut h=0.8d.; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °CZinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
Minimum Service Temperature, Air -55.0 °CZinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
Flash Point >= 100 °Cuncured
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 3.00 hourFunctional Cure. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
 5.00 - 10.0 hourFull Cure. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
 20.0 - 40.0 minHandling, Cured. Zinc plated bolt M 10x20- quality 8.8- nut h=0.8d.
Shelf Life 12.0 Month
@Temperature <=28.0 °C
uncured
 
Descriptive Properties
Chemical ClassAnaerobic Methacrylate
Color / appearancewhite
Locking Torque2-4 N.m. Prevailing. ISO 10964. Zinc Plated bolt M 10x20 quality 8.8-nut h=0.8d
 7-10 N.m. Breakaway. ISO 10964. Zinc Plated bolt M 10x20 quality 8.8-nut h=0.8d

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9184 / 233550

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.