MB2000-5 is an excellent flame and track resistant material possessing outstanding electrical and mechanical properties. The 2000 Series’ good dielectric strength and low shrink allow close dimensional control. Key features include Rated UL 94 V0 @1.5mm. UL file number E80533 Information provided by Mar-Bal, Inc. |