MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crystex Composites Mycalex Insulators® MM 50-U-100 Stand Off Insulator
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Produced from Mycalex MM 451 glass mica ceramic. Inserts: Nickel Plated carbon steel or AISI 316 Stainless steel are standard; other materials available per request. Manufactured by transfer molding.

Used for stand-off insulators and brush holders for the rail transportation, power generation, and traction motor industries. All parts are RoHS and Reach compliant (lead-free). Mycalex Insulators are made from inorganic materials that do not burn. Compliant to EN 45545-2, NF F16-101 and NF-F-102.

Typical data below provided by Crystex Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 150 MPa>= 21800 psi
Flexural Strength >= 45.0 MPa>= 6530 psi
Compressive Strength >= 500 MPa>= 72500 psi
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 2.00e+11 ohm>= 2.00e+11 ohm1000V
Dielectric Breakdown >= 26000 V>= 26000 VArc Over Voltage (Air)
 >= 30000 V>= 30000 VBreakdown Voltage (Air)
Comparative Tracking Index >= 600 V>= 600 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 450 °C842 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
Capacitance6.5 pF
Torsion> 90 N-m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMYKROY978 / 268810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.