MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nilit Polynil® P50FIL Super Fast Cycling, Nucleated Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Nucleated

Material Notes: Description: Polynil P50 FIL is a nucleated, internally lubricated NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production articles that require fast cycle times, like lighter bodies, aerosol sprays and terminal blocks.

Key characteristics:

  • Excellent flow
  • Fast cycle time
  • High elongation
  • Good mould release
  • High toughness
  • Good thermal performance

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.5 %24h in H2O; sim. ISO 62
Water Absorption at Saturation 8.5 %sim. ISO 62
Loss On Ignition 28 %ASTM D2863
Viscosity Measurement 50relative viscosity (formic acid); ASTM D789
Linear Mold Shrinkage, Flow 0.011 cm/cmNilit
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12600 psiASTM D638
Elongation at Break 35 %ASTM D638
Flexural Strength 18000 psiASTM D790
Flexural Modulus 424 ksiASTM D790
Izod Impact, Notched (ISO) 1.90 ft-lb/in²ASTM D256
Charpy Impact Unnotched NBISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 457 V/mil
@Thickness 2.00 mm
ASTM D149
Comparative Tracking Index >= 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 162 °FASTM D648
Flammability, UL94 V-2
@Thickness 0.800 mm
 V-2
@Thickness 1.60 mm
 
Descriptive Properties
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLBN09 / 50398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.